Study on contact corrosion characteristics of metal down lead and flexible graphite
Author:
Affiliation:

1. Henan SIDA Power Equipment Co., Ltd Xu Chang 461500,China;2. School of electrical engineering, Zhengzhou University, He Nan, 450000,China;3. Department of Electrical Engineering,Xing tai Polytechnic College,Hebei,054000,China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为验证石墨基柔性接地装置中石墨基柔性接地体对金属引下线腐蚀行为的影响。通过对镀锌板、铜金属、304不锈钢三种金属与石墨材料连接后进行模拟土壤包覆、强电解质土壤通电流等不同类型的加速腐蚀试验,并采用失重法、XRD以及极化曲线等方法,研究不同加速腐蚀试验类型对镀锌板、铜、不锈钢三种金属腐蚀行为的影响。结果表明:几种金属材料与石墨材料连接后的耐蚀顺序依次为304不锈钢>铜金属>镀锌钢,硫酸根离子浓度的增加会加速石墨接地材料对金属接地材料的腐蚀。结论为石墨基柔性接地装置中引下线优选304不锈钢或304不锈钢与石墨复合材,镀锌钢表面的腐蚀产物具有明显的层状结构,内层腐蚀产物主要为Zn5(OH)8Cl2H2O、Fe4(OH)10SO4,外层腐蚀产物的含氧量高,质地较疏松,主要为SiO4和Zn。

    Abstract:

    Objective to verify the influence of graphite based flexible grounding body on Corrosion Behavior of metal down lead in graphite based flexible grounding device. Methods three kinds of accelerated corrosion tests were carried out to simulate soil coating, strong electrolyte soil current and other types of accelerated corrosion tests after connecting galvanized sheet, copper metal and 304 stainless steel with graphite material. The influence of different accelerated corrosion test types on Corrosion Behavior of galvanized sheet, copper and stainless steel was studied by weight loss method, XRD and polarization curve. Results the order of corrosion resistance was 304 stainless steel > copper metal > galvanized steel. The increase of sulfate ion concentration would accelerate the corrosion of graphite grounding materials to metal grounding materials. Conclusion 304 stainless steel or 304 stainless steel and graphite composite material is preferred for down lead of graphite based flexible grounding device, the corrosion products on the surface of galvanized steel have obvious layered structure, the main corrosion products of inner layer are Zn5(OH)8Cl2H2O, Fe4(OH)10SO4, and The outer corrosion products have high oxygen content and loose texture, mainly SiO4 and Zn.

    参考文献
    相似文献
    引证文献
引用本文

张国锋,李景丽,李孟.金属引下线与柔性石墨接触腐蚀特性研究[J].电子测量技术,2021,44(3):16-21

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2024-12-19
  • 出版日期:
文章二维码
×
《电子测量技术》
财务封账不开票通知